ASA and ABS filaments: outdoor and heat-resistant parts – how to print without warping
PLA is great for prototypes and decorative items, but in sunlight or near a warm machine it quickly softens and deforms. When a part must withstand heat, impacts or outdoor conditions – a car mount, an engine cover, an outdoor housing – ASA or ABS is usually chosen ASA or ABS. Both filaments are tougher and more heat-resistant than PLA, but harder to print: without the right conditions, corners lift off the plate and tall parts crack between layers. In this article – how they differ and how to print them without failures.
ASA vs ABS – what's the difference
| ASA | ABS | |
|---|---|---|
| UV and weather resistance | very good – designed for outdoor parts | moderate – fades and becomes brittle outdoors over time |
| Heat resistance | high (Bambu Lab ASA: 92 °C per ISO 75, 1.8 MPa) | high, similar to ASA |
| Impact resistance | good | good |
| Odour when printing | noticeable | strong, pungent |
| Where to use | outdoor mounts, car parts, housings in sunlight | indoor parts: housings, brackets, tool parts, mechanical components |
Simple rule: if the part will be outdoors or in sunlight – ASA; if indoors – ABS is also fine. When you need even more stiffness, reinforced variants are available, e.g., Polymaker Fiberon ASA-CF08 with carbon fibre or Rosa3D ASA + 5 % Kevlar. If the housing requires flame retardancy – Rosa3D ABS V0 FR (more in the article about V0 filaments).
What printer you need
The most important requirement is an enclosed chamber. ASA and ABS shrink strongly as they cool; if cold room air moves around the part, the upper layers cool faster than the lower ones and the part starts to curl or crack. In the Bambu Lab filament table, ABS and ASA are not recommended for open printers (A1, A1 mini) not recommended, while for enclosed printers they are recommended. Suitable, e.g., Bambu Lab P1S, P2S ar H2S.
A hardened nozzle is not needed for plain ASA and ABS – a standard brass one is enough. It is only required for fibre-reinforced filaments (CF, GF) – see CF filaments.
Recommended settings
Manufacturer-specified ranges (per the Bambu Lab filament table and the ASA technical data sheet):
| Parameter | ASA | ABS |
|---|---|---|
| Nozzle temperature | 240–270 °C (data sheet), 240–280 °C (filament table) | 240–280 °C |
| Bed temperature | 90–100 °C | 90–100 °C |
| Plate | Textured PEI, Engineering, High Temp + glue | Textured PEI, Engineering, High Temp + glue |
| Part cooling fan | 0–80 % | 0–80 % |
| Drying | 80 °C, 8 h (in a drying oven) | 80 °C, 8 h |
Bambu Studio and other software already include ready-made profiles for original filaments (Bambu Lab ASA, Bambu Lab ABS) – start with those. For other manufacturers' filaments (Polymaker ASA, Polymaker ABS) always check the temperature on the spool label.
How to avoid warping: 8 tips
- Close the chamber and heat it up. Before printing, let the bed warm the air in the chamber for 5–10 min. Do not open the door or top cover.
- Use glue. Bambu Lab recommends printing ASA and ABS with glue – glue stick or liquid glue. It helps adhesion and protects the plate surface.
- Keep the plate clean. Fingerprint oils are the most common reason corners lift. Textured PEI plate: wash with warm water and dishwashing liquid.
- Add a brim (a border) – especially for long, flat parts and parts with sharp corners. Bambu Lab recommends it for ABS.
- Reduce cooling. Strong airflow causes layers to separate. For tall parts, use a lower fan speed.
- Avoid draughts. Do not place the printer near a window, door or air conditioner.
- Round off corners in the model. Sharp 90° corners lift the most; even a small rounding helps.
- Dry the filament. Damp filament bubbles, the surface becomes rough and layer adhesion weakens. Store it sealed with a desiccant bag (more in about drying and storing filament).
Safety: odour and ventilation
ABS and ASA release a pungent smell when printed – the Bambu Lab ABS filament description states that an enclosed chamber is required because of the odour. Keep the printer in a well-ventilated room, not a bedroom, and after printing wait for the chamber to cool before opening the door. In a business setting, it is worth placing the printer in a separate, ventilated area.
Part after printing
- Remove the part only once it has cooled – a hot part may deform when bent.
- Annealing. Bambu Lab recommends 80–90 °C for 6–12 hours – this can increase heat resistance, but the part may change slightly. The manufacturer warns against using a household oven or microwave oven.
- Strength depends not only on the filament, but also on wall thickness, infill and part orientation – see 3D printed part strength.
How to find them on inteq.lt
You will find ASA, ABS and other engineering filaments in the category Filaments, plates – Build plates. If you are not sure which filament to choose for a specific part, first read which filament to choose for spare parts or write to us via užklausos formą – we will advise.